What grit progression does Jim Kibler recommend for sanding a buttplate after filing?

A typical progression is 150 grit over the whole part, then 220 grit over the whole part, then 320 grit over the whole part. The whole process takes roughly 15 to 20 minutes once you are moving through the grits.